                        Composition chimique:6% à 8% de zinc
Force de fatigue:Bien
Conductivité électrique:33% SIGC
Thermal Conductivity:130 W/mK
Tensile Strength:83,000 Psi
Shape:Round
Shear Strength:48,000 Psi
Yield Strength:73,000 Psi
Fatigue Strength:Good
Application:Aerospace, Defense, Shafts, Gears
Thermal Conductivity:130 W/mK
Chemical Composition:6%-8% Zinc